Shaoxing Tianlong Tin Materials Co.,Ltd.
Shaoxing Tianlong Tin Materials Co.,Ltd.
Sn25Zn75 for Film-Capacitor Metal-Spray
  • Sn25Zn75 for Film-Capacitor Metal-Spray
Sn25Zn75 for Film-Capacitor Metal-Spray

Sn25Zn75 for Film-Capacitor Metal-Spray

Payment Type:
L/C, T/T
Incoterm:
FOB, CIF
Delivery Time:
15 Days
Transportation:
Ocean, Land, Air
Port:
SHANGHAI, NINGBO
Quantity:

Your message must be between 20 to 2000 characters

Contact Now
Basic Info
Basic Info
Place of Origin: SHAOXING,CHINA
Productivity: 60TON PER MONTH
Supply Ability: 120TON PER MONTH
Payment Type: L/C,T/T
Incoterm: FOB,CIF
Certificate: ISO9001
HS Code: 79040000
Transportation: Ocean,Land,Air
Port: SHANGHAI,NINGBO
Product Description
Product Description


The Sn25Zn75 Tin Zinc alloy wires have good mechanical strength and solderability. They can provide spraying metal layer of Film Capacitor Metal Spray ,with strong adhesion ability, and give capacitors good electrical performance, such as reduced loss angle. They comply with EU RoHS and WEEE directives on lead-free electronic products, as well as the requirements of ISO 14000 system.

 

1. APPLICATION

  THE WIRE COULD BE SPRAYED ON THE SURFACE OF FILM CAPACITORS

 

2.  SPECIFICATION

2-1. APPEARANCE

     THE WIRE MUST BE CHECKED THE CONDITIONS(CRACK, BURR, CORROSION & OTHER DEFECTS) OF THE SURFACE BY SIGHT, AS A DETERMINTAL TO USE.

 

2-2. DIAMETER : 1.1~3.2mm   

DIAMETER(MM)

TOLERANCE

DIAMETER(MM)

TOLERANCE

1.1≤Ф≤1.65

+0.00~0.03

2.00Ф≤2.30

+0.00~0.05

1.65Ф≤2.00

+0.00~0.04

2.30Ф≤3.20

+0.00~0.06

2-3. CHEMICAL COMPOSITIONS(%)

SPECIFICATION

MAIN INGREDIENT(%)

IMPUTIRY(%)≤

Sn

Zn

Pb

Cd

Fe

HYSnZn10

89.00~91.00

9.00~11.00

0.04

0.002

0.012

0.05

HYSnZn15

84.00~86.00

14.00~16.00

0.04

0.002

0.012

0.05

HYSnZn20

79.00~81.00

19.00~21.00

0.04

0.002

0.012

0.05

HYSnZn30

69.00~71.00

29.00~31.00

0.04

0.002

0.012

0.05

HYSnZn40

59.00~61.00

39.00~41.00

0.04

0.002

0.012

0.05

HYSnZn50

48.00~52.00

48.00~52.00

0.04

0.002

0.012

0.05

HYSnZn60

38.00~42.00

58.00~62.00

0.04

0.002

0.012

0.05

HYSnZn70

28.00~32.00

68.00~72.00

0.04

0.002

0.012

0.05

HYSnZn75

23.00~27.00

73.00~77.00

0.04

0.002

0.012

0.05

HYSnZn80

18.00~22.00

78.00~82.00

0.04

0.002

0.012

0.05

 

2-4. PHYSICAL PROPERTIES & MECHANICAL PROPERTIES

     MELTING POINT : 198~390℃

     GRAVITY : 7.0~7.3 g/cm2

     ELONGATION(%) : ≥20 A100mm(%)

     TENSILE STRENGTH : ≥60 Rm(N/mm2)

   VOLUME RESISTIVITY: ≤76 mΩ.mm2/m at 20℃

Tin zinc alloy wire


Send your message to this supplier

  • Ms. kathy

  • Enter between 20 to 4,000 characters.